Micro-foaming agentMicro-cells invisible to the eye · food-contact grade
A new micro-foaming agent developed to replace conventional plastic filler masterbatch — the micro-foaming filler masterbatch offsets the effect of filler masterbatch on plastic density (specific gravity), cutting production cost more effectively.
- Density @25 ℃
- 0 – 0
- pH value
- 0 – 0
- Gas yield
- 0 – 0 mL/g
- Released gas
- CO₂ · non-toxic
Cell cross-section: conventional filler vs micro-foamed
Toggle the comparison: conventional filler masterbatch gives a dense matrix with white/black speck defects; F818 micro-foaming gives even micro-cells invisible to the eye, defect-free, with adjustable density.
Insulation improved by more than 50%
Compared with conventional filler masterbatch, the micro-foaming filler masterbatch used in agricultural film improves thermal insulation by more than 50%.
Handfeel · rigidity · heat-seal all restored
Too much conventional calcium carbonate filler causes a poor handfeel and lack of rigidity; too much talc damages heat-seal performance. The micro-foaming filler masterbatch largely eliminates this whole set of defects.
Density adjustable down to 10% below the original plastic
In profiles, thermal deformation is 60% better than conventional filler masterbatch; depending on the required specific gravity the density can match the plastic or even drop 10% below the original plastic.
Specification and safety
A COA test report accompanies every batch; non-toxic and harmless, meeting food-contact grade.
Main uses · performance · applications
Micro-cells invisible to the eye; no white or black specks when blown into film; lower cost, higher efficiency.
Main use
Mainly for micro-cellular foaming invisible to the eye in plastics, to make micro-foaming filler masterbatch and similar.
Appearance and processing
Excellent dispersion; after film blowing the surface has no white or black specks, the fineness is high and the product shows good gloss and toughness.
Lower cost, higher efficiency
Effectively improves the overall performance of plastic products and markedly reduces material usage and production cost.
Plastic film
Woven sacks
Density control range (relative to the original plastic · 80 – 105% scale)
Recommended dosage 0.5% – 1.5% · Packaging 25 kg / drum
Request an F818 sample
01Product positioning
Name and positioning. The data page is titled "Microfoaming agent F818"; the application field section records "used for processing plastic films, trash bags, shopping bags, vest bags, packaging bags, etc." Main use: "mainly used for microcellular foaming invisible to the naked eye in plastics, microfoamed filler masterbatch, etc." (Data source: product handbook)
Overview (verbatim excerpt): "Microfoaming agent F818 is a microfoaming agent developed by our company according to market needs to change conventional plastic ordinary filler masterbatch. For example, the microfoamed filler masterbatch produced by adding the microfoaming agent on the basis of ordinary filler masterbatch production compensates for the effect of filler masterbatch on plastic density (specific gravity) and more effectively reduces production costs. Compared with ordinary filler masterbatch, the thermal insulation performance of microfoamed filler masterbatch used in agricultural film is 50% better. Another example is for packaging films: adding too much ordinary calcium carbonate filler masterbatch affects the hand feel and makes it lose rigidity; adding too much talc filler masterbatch affects heat-sealing performance. Microfoamed filler masterbatch almost compensates for this series of defect problems. For profiles, the heat deformation rate is 60% better than that of ordinary filler masterbatch; according to product specific gravity requirements, it can be adjusted to the same specific gravity as the plastic or even a specific gravity 10% lower than that of the original plastic." (Data source: product handbook)
Application and performance section (verbatim excerpt): "Used for processing plastic films, trash bags, shopping bags, vest bags, packaging bags, etc. It has very good dispersibility; blown film has no white spots or black spots; fineness is high; the product has good gloss and toughness. Mainly suitable for filling modification of woven bags, strapping, hollow articles, pipes, sheets, and injection-molded products; it can improve the performance of plastic products and greatly reduce product cost." (Data source: product handbook)
Key technical indicators: appearance and odor "white viscous flowable ether-smelling liquid"; density 1.28-1.30; PH value 8-8.3; gas evolution 45-48 ml·g⁻¹; decomposition temperature 160℃; released gas "carbon dioxide". (Data source: product handbook)
- Gas evolution characteristics: decomposition temperature 160℃, released gas is carbon dioxide; gas evolution 45-48 ml·g⁻¹.
- Performance statement (verbatim): It has very good dispersibility; blown film has no white spots or black spots; fineness is high; the product has good gloss and toughness.
- Toxicity clause (verbatim excerpt): "Non-toxic and harmless, complies with food-contact grade standards." — verbatim; for relevant compliance, the documents supplied with the goods shall prevail.
- This grade is a historically listed grade (Discontinued); the documentation is retained; this page is compiled as-is from historical data.
02Formulation system & mechanism of action
Gas evolution pathway. The documentation records that this product releases carbon dioxide at a decomposition temperature of 160℃, with a gas evolution of 45-48 ml·g⁻¹—the gas forms microcells invisible to the naked eye within the system. (Data source: product handbook)
Composite system. This product is added on the basis of conventional plastic ordinary filler masterbatch to prepare "microfoamed filler masterbatch"; the microcellular structure compensates for the effect of filler masterbatch on plastic density (specific gravity) and reduces production costs. (Data source: product handbook)
Performance-related statement (verbatim): when used in films, "it has very good dispersibility; blown film has no white spots or black spots; fineness is high; the product has good gloss and toughness"; it covers filling modification applications such as bags, woven bags, strapping, hollow articles, pipes, sheets, and injection-molded products. (Data source: product handbook)
- Mixing in — microfoamed filler masterbatch systemAdd the microfoaming agent on the basis of ordinary filler masterbatch to prepare microfoamed filler masterbatch.
- Gas evolution — carbon dioxide microcell formationAfter the processing temperature reaches the decomposition temperature of 160℃, carbon dioxide is released, forming microcells invisible to the naked eye.
- Specific gravity setting — balancing cost reduction and performanceAdjust the microcell ratio according to specific gravity requirements; the documentation records improved thermal insulation for agricultural film, and specific gravity can be adjusted to be 10% lower than that of the original plastic.
03Key parameters
The table below summarizes the main components and physicochemical properties of F818 recorded in the documentation (original wording and units from the documentation are retained).
| Item | Value / description |
|---|---|
| Main component | Microfoaming agent |
| Appearance and odor | White viscous flowable liquid with an ether odor |
| Density | 1.28-1.30 |
| pH | 8-8.3 |
| Gas evolution | 45-48 ml/g |
| Decomposition temperature | 160 °C |
| Released gas | Carbon dioxide |
| Toxicity | Non-toxic and harmless, conforms to food-contact grade standards |
The entry for this grade does not list prohibited items or special tests; toxicity clauses are reproduced verbatim (see Section 7); items not recorded in the documentation do not appear in this table. (Data source: product handbook / official product data)
04Recommended dosage window
The documentation gives one range for the addition of this product:
| Scenario | Dosage | Conditions & notes |
|---|---|---|
| Dosage | 0.5%-1.5% | Source text: '[Dosage] 0.5%-1.5%'; the denominator is not specified (reproduced verbatim; not inferred). |
The documentation gives only one range and does not specify the denominator; it is presented verbatim, and the denominator is not inferred. The value to use within this range should be determined by small-scale trials according to the masterbatch formulation and target specific gravity.
This entry is the only dosage record for this grade in the documentation; there is no second line item and no scenario-specific tiering; this page does not infer a denominator and does not perform cross-grade conversion. (Data source: product handbook)
05Applications
The documentation lists the following application areas:
- Plastic films
- Agricultural films, packaging films, and other areas; blown films have no white spots or black spots, with good gloss and toughness (as stated in the documentation).
- Bag products
- Garbage bags, shopping bags, vest bags, packaging bags.
- Filling modification
- Filling modification of woven bags, strapping, hollow articles, pipes, sheets, and injection-molded products; can improve the performance of plastic products and reduce product cost (as stated in the documentation).
06How it differs from related grades
F818 and ACM750 both belong to the microfoaming field and are commonly used as a pair; the two grades differ in released gas and technical specifications, so select according to the target. The comparison is as follows:
| Grade | Source positioning (key points) | Key technical specifications | Dosage (documented) |
|---|---|---|---|
| F818 | Microfoaming agent developed by changing the conventional plastic ordinary filled masterbatch approach; "specific gravity 10% lower than that of the original plastic"; used in film and bag applications | Appearance: white viscous flowable liquid with ether odor; gas evolution 45-48 ml·g⁻¹; decomposition temperature 160℃; released gas: carbon dioxide | 0.5%-1.5% |
| ACM750 | Microfoaming agent that changes plastic weight; "for profiles, the heat deformation rate is 60% better than that of ordinary filled masterbatch"; specific gravity can be adjusted to 15% lower than that of the original plastic | Appearance: yellow viscous flowable liquid with ether odor; gas evolution 75-96 ml·g⁻¹; decomposition temperature 160℃; released gas: nitrogen; molecular weight 6500-7300 | 0.5%-10% |
Reading note: both grades are in the microfoaming field, but the released gas (carbon dioxide / nitrogen), gas evolution, and dosage ranges differ; values cannot be applied interchangeably. (Data source: product handbook)
Replacement & selection
For selection and replacement evaluation after discontinuation, refer to the following in-production information:
Replacement guidance: official documentation does not publish a direct replacement for this grade; according to the site's existing wording, "for replacement selection, see same-series listed models"; the current in-production catalog has no same-use (microfoaming) grade; a selection entry is provided below.
- Product Overview (in-production grades)Selection entryBrowse in-production grades by processing scenario (film / bags / filling modification) for replacement evaluation.
Note: for replacement evaluation, combine with small-scale system trials; the dosage basis of the comparison grade differs from that of this grade, and values cannot be applied interchangeably. (Data source: product handbook / official product data)
07Usage & storage
The following points are taken item by item from documented records; items not listed in the documentation are not drafted on our behalf.
Documented records (verbatim)
- Technical specifications: appearance and odor "white viscous flowable liquid with ether odor"; density 1.28-1.30; pH value 8-8.3; gas evolution 45-48 ml·g⁻¹; decomposition temperature 160℃; released gas "carbon dioxide".
- Toxicity clause (verbatim): "Non-toxic and harmless, complies with food-contact grade standards."
- Dosage (verbatim): 0.5%-1.5%.
- Packaging: 25 kg/drum.
Not in the documentation (not drafted on this page)
- This grade's entry does not list storage conditions, shelf life, prohibited items, or safe handling data (MSDS level)—the existing documentation does not record them.
08FAQ
What is F818?
Microfoaming agent: microfoaming filled masterbatch is prepared on the basis of conventional plastic ordinary filled masterbatch, reducing the effect of filled masterbatch on plastic density and production cost; the documentation records that agricultural film thermal insulation performance is 50% better than ordinary filled masterbatch, profile heat deformation rate is 60% better, and specific gravity can be adjusted to 10% lower than that of the original plastic. (Data source: product handbook)
What is the dosage? What is the denominator?
Original documentation: "[Dosage]0.5%-1.5%"; the denominator is not stated—this page records it verbatim and does not draft a denominator. For values within the range, determine them by small-scale trials according to the masterbatch formulation and target specific gravity. (Data source: product handbook)
How is it distinguished from ACM750?
Both grades are in the microfoaming field: F818 releases carbon dioxide (gas evolution 45-48 ml·g⁻¹), and the documentation records its use in film, bag, and filling modification applications; ACM750 releases nitrogen (gas evolution 75-96 ml·g⁻¹). The dosage ranges differ, and values cannot be applied interchangeably. (Data source: product handbook)
What is the current status of F818?
F818 has been listed as a Discontinued grade (documentation retained). This page's content is compiled verbatim from historical documentation and is not a recommendation for a product for sale; for selection, refer to current in-production grades and the latest documentation. (Data source: official product data)
What is the replacement grade for F818?
Official documentation does not publish a direct replacement grade; the current in-production catalog has no same-use grade—you can screen in-production grades by processing scenario via the Product Overview for replacement evaluation (see the entry link in Section 6, "Replacement & Selection").
Can F818 still be purchased? Is it in stock?
This grade has been listed as a Discontinued grade (documentation retained). This page is not published as on-sale information; for supply and selection, refer to current in-production grades and official information.
Why is F818 discontinued?
Reason for discontinuation: not recorded in the existing documentation (not drafted on this page).
AppendixData sources
The data on this page come from product documentation and are traceable item by item:
- Product handbook: F818 entry (overview / technical specifications / toxicity / main uses / application fields / dosage / packaging); comparison section in the same handbook (ACM750 entry).
- Cross-verification of documentation: for the same grade entry, excerpts are consistent across three documents—the handbook, the comprehensive series volume, and the content-edited version (single source family; three volumes cross-verify).
Not covered by the source material (not written on this page — to be added later)
- Dosage denominator: not stated in the documentation ⇒ this page records the range verbatim and does not draft a denominator.
- Food-contact grade statement: taken from the original documentation (verbatim); for relevant compliance, refer to the documents accompanying the shipment.
- Storage conditions, shelf life, prohibited items, and safe handling data (MSDS level): not recorded in the existing documentation.
F818 is listed as a discontinued grade; the documentation is retained. This page is compiled from historical source material and is not a recommendation of a currently supplied product; please base your selection on current production grades and the latest documentation.